Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Addcomp ADD-VANCE® THC 453 PP based masterbatch containing heat stabilizers and carbon black

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Addcomp
Trade Name ADD-VANCE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Addcomp ADD-VANCE® THC 453 PP based masterbatch containing heat stabilizers and carbon black.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Fields of application: Stabilization masterbatch for producing long fiber reinforced polypropylene for D-LFT processExamples: Long fiber reinforced pellets to be used for automotive parts, like underbody panels and shields, structural parts, etc. Mode of action and advantages: ADD-VANCE® THC 453 contains a combination of heat stabilizers and carbon black. Heat stabilizers inhibit the thermo-oxidative degradation by radical scavenging and decomposing reactive hydroperoxides.Advantages: Excellent Long Term Heat Ageing (LTHA) performance to achieve VW and D-C requirements. The minimum long term heat ageing will be 1200 hours @ 150 deg. Celsius applying 2 or 2,6% dosing level on PP, depending on the glass concentration, please see page 2); Excellent mechanical properties after heat-aging (D-C test method); Good glueing properties; High accuracy in dosing of each individual additive component in ADD-VANCE® THC 453 to ensure product consistency and a guaranteed stabilization of end-product; Optimized additive formulation to achieve lower overall additivation costs and easy processing; Non-sticking pellets, dust free dosing; and Safe and easy handling.Information provided by ADDCOMP
Physical Properties Metric English Comments
Bulk Density 0.500 - 0.650 g/cc
0.0181 - 0.0235 lb/in³
Processing Properties Metric English Comments
Processing Temperature <= 300 °C
<= 572 °F
Descriptive Properties Value Comments
Appearance Black granules
Dosing Level 0.02
for LFT containing 20-30% glass
0.026
for LFT containing 40% glass
Users viewing this material also viewed the following: