| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | ASTM D4895 |
|
3M Dyneon™ TF 2072 PTFE
(discontinued **)
Processable by standard paste extrusion methodTF 2071 and TF 2072 have a wide processing range because of high maximum allowable reduction ratioTF 2072 is recommended for thin-wall, small diameter t..
|
|||
| Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | Tap Density |
|
Momentive Performance Materials AC6103 Boron Nitride (BN) Powder
Agglomerate of hexagonal BN crystals. AC6103 powders are granular with good flow and blend characteristics as well as high thermal conductivity and good lubrication qualities. Information provided..
|
|||
| Bulk Density | 0.500 - 1.20 g/cc | 0.0181 - 0.0434 lb/in³ | Apparent Density |
|
Indium Corp. Fine ITO Indium Tin Oxide
Indium Tin Oxide (ITO, or tin-doped indium oxide) is a mixture of indium(III) oxide and tin(IV) oxide, typically 90% indium oxide, 10% tin oxide by weight. In powder form it is yellow-green in colo..
|
|||
| Bulk Density | 0.500 - 0.700 g/cc | 0.0181 - 0.0253 lb/in³ | |
|
Solvay Chemicals Ixper® 25M Magnesium Peroxide
IXPER® 25M is a Magnesium Peroxide powder used in a wide range of applications in environmental, and oil drilling e.g. markets. EINECS Number: 215-627-7/CAS Number: 1335-26-8Information provided ..
|
|||
| Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | Dried at 110°C |
|
Sharadaa Ceramics REFINSUL 4 Insulating Castables Medium/High Purity
Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan..
|
|||
| Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | |
|
Solvay SOPROPHOR® K/202 Surfactant
Description: Multipurpose dispersing agent for SC formulationsIdentification: ABSORBED SURFACTANTSolubility: Dispersible in water. Insoluble in polar and aromatic solvents.Available in: Asia Pacific..
|
|||
| Bulk Density | >= 0.500 g/cc | >= 0.0181 lb/in³ | |
|
Chosun Refractories LW-20 Special Insulating Firebrick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
|
|||
| Bulk Density | >= 0.500 g/cc | >= 0.0181 lb/in³ | |
|
Chosun Refractories A-1 Insulating Firebrick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
|
|||
| Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | |
|
Chosun Refractories CFA-1 Ceramic Foam
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
|
|||
| Bulk Density | 0.500 - 0.650 g/cc | 0.0181 - 0.0235 lb/in³ | |
|
Addcomp ADD-VANCE® NU 489 Nucleation masterbatch, PP based
Fields of application: Extruded and injection molded articles made from PP resins.Examples: Extruded PP sheets, films, tapes and blow molded and injection molded articles, such as garden furniture, ..
|
|||
| Bulk Density | 0.500 - 0.650 g/cc | 0.0181 - 0.0235 lb/in³ | |
|
Addcomp ADD-VANCE® TH 130 Stabilization Masterbatch, PP base
Fields of application: Stabilization and processing master batch for producing glass mat reinforced polypropylene (GMT) and long fiber reinforced PP materials (LFTs).Examples: Long fiber reinforced ..
|
|||
| Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
|
BASF Ultramid® 1C PA6/66 (Conditioned)
Description: Ultramid® 1C forms flexible, scratch-resistant coatings or tough, resilient, abrasion-resistant coverings on plastics, films, nonwovens, fabrics, leather, paper, wood, or metal.Informa..
|
|||
| Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
|
BASF Ultramid® 1C PA6/66 (Dry)
Description: Ultramid® 1C forms flexible, scratch-resistant coatings or tough, resilient, abrasion-resistant coverings on plastics, films, nonwovens, fabrics, leather, paper, wood, or metal.Informa..
|
|||
| Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
|
BASF Ultramid® A3EG10 50% Glass Filled PA66 (Conditioned)
Description: 50% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness as well as for electric insulating parts.Information provided by BASF
|
|||
| Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
|
BASF Ultramid® B3EG5 25% Glass Filled PA6 (Dry)
Description: 25% glass-fiber reinforced injection-molding grade for industrial articles and electrical insulating partsInformation provided by BASF
|
|||
| Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
|
BASF Ultramid® B3EG7 35% Glass Filled PA6 (Conditioned)
Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF
|
|||
| Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
|
BASF Ultramid® KR 4355 G10 BK 23215 50% Glass Filled PA6/6T (Conditioned)
Description: 50% glass-fiber reinforced product for injection molding; high toughness and rigidity; low water absorption, high melting point (285°C); mechanical properties remain constant up to 60°..
|
|||
| Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
|
BASF Ultramid® KR 4355 G7 BK 00564 35% Glass Filled PA6/6T (Dry)
Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r..
|
|||
| Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
|
BASF Ultramid® KR 4365 G5 BK 00100 35% Glass Filled PA6/6T FR (Conditioned)
Description: Partially aromatic polyamide; flame retardant based on red phosphorus; low water absorption, high melting point (295°C); low tendency to form deposits on electrical contacts, very resi..
|
|||
| Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | |
|
Asahi Glass Fluon® CD145 PTFE Coagulated Dispersion Powder
Fluon®PTFE coagulated dispersion powders (fine powders) are used for paste extrusion to make tapes, tubes, rods and wire coatings.Information provided by Asahi Glass Company, Inc.
|
|||
| Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
|
BASF Ultramid® B35EG3 15% Glass Filled PA6 (Conditioned)
Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat..
|
|||
| Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
|
BASF Ultramid® B35G3 BK 00564 15% Glass Filled PA6 (Dry)
Description: 15% glass fiber reinforced injection molding grade e.g. for internal gas pressure applications such as flashing direction switch gears, automobile mirror housings and wheels of mountain..
|
|||
| Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
|
BASF Ultramid® B3GK24 BK 00564 10/20% Glass/Glass Bead Filled PA6 (Conditioned)
Description: combined 10% glass-fiber and 20% glass-bead reinforced injection-molding grade for technical articles of very good dimensional stability, for instance, vehicle ash tray housings and ele..
|
|||
| Bulk Density | 0.500 - 0.650 g/cc | 0.0181 - 0.0235 lb/in³ | |
|
Addcomp ADD-VANCE® NU 559 Nucleation masterbatch, PP based
Fields of application: Extruded and injection molded articles made from PP and PE resins.Examples: Extruded sheets, films, tapes and blow molded, compression molded and injection molded articles, su..
|
|||
| Bulk Density | 0.500 - 0.600 g/cc | 0.0181 - 0.0217 lb/in³ | |
|
Borealis RB206MO-06 Polypropylene Random Copolymer
RB206MO-06 is a random copolymer with good transparency and contact clarity, very good gloss and surface finish. The high stiffness of this grade allows for a reduction in cycle time. This grade als..
|
|||
| Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
|
BASF Ultramid® B3UG4 Grey 22975 20% Glass Filled PA66 FR (Dry)
Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire..
|
|||
| Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
|
BASF Ultramid® B3WG10 BK 00564 50% Glass Filled PA6 (Conditioned)
Description: 50% glass-fiber reinforced and heat aging resistant injection-molding grade for technical parts with very high stiffness.Information provided by BASF
|
|||
| Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
|
BASF Ultramid® B3WG10 BK 00564 50% Glass Filled PA6 (Dry)
Description: 50% glass-fiber reinforced and heat aging resistant injection-molding grade for technical parts with very high stiffness.Information provided by BASF
|
|||
| Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
|
BASF Ultramid® Seal-Fit PA6/66 (Conditioned)
Description: Transparent, tough, amorphous copolyamide for injection molding, specially developed for tight overmoulding of metal inlays.Information provided by BASF
|
|||
| Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
|
BASF Ultramid® B3WG5 25% Glass Filled PA6 (Dry)
Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el..
|
|||