Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Albis Plastics Tedur® L 9511 PPS, 45% Glass Fiber

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler
Manufacturer Albis Plastics
Trade Name Tedur®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Albis Plastics Tedur® L 9511 PPS, 45% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
High Strength, High Rigidity Standard Grade. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Fixture Elements, HousingsProcessing: Injection Molding (Melt Temperature: 610-645°F, Mold Temperature: 285°F)Tedur® is manufactured by Albis Plastics Corporation under license of the registered trademark owner (Bayer.) Data supplied by Albis Plastics Corporation.
Physical Properties Metric English Comments
Density 1.74 g/cc
0.0629 lb/in³
DIN 53 47
Mechanical Properties Metric English Comments
Tensile Strength at Break 170 MPa
24700 psi
DIN 53 455
Elongation at Break 1.4 %
1.4 %
DIN 53 455
Modulus of Elasticity 16.5 GPa
2390 ksi
DIN 53 457
Flexural Yield Strength 250 MPa
36300 psi
DIN 53 452
Flexural Modulus 15.0 GPa
2180 ksi
DIN 53 457
Izod Impact, Notched 2.99 J/cm
5.60 ft-lb/in
Approximation; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 260 °C
500 °F
ASTM D648
Flammability, UL94 V-0
V-0
Processing Properties Metric English Comments
Melt Temperature 321 - 341 °C
610 - 646 °F
Injection
Mold Temperature 141 °C
286 °F