| Category | Metal , Electronic/Magnetic Alloy , Nonferrous Metal , Cobalt Alloy , Nickel Alloy |
| Manufacturer | Alliance LLC |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Alliance A-5-7 Alnico Magnetic Material.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 7.30 g/cc | 0.264 lb/in³ |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Vickers | 450 - 700 | 450 - 700 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 11.0 - 13.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 7.22 µin/in-°F @Temperature 68.0 °F |
Parallel DOM |
| Maximum Service Temperature, Air | 525 °C | 977 °F |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 0.0000470 - 0.0000530 ohm-cm | 0.0000470 - 0.0000530 ohm-cm | |
| Magnetic Coercive Force, Hc | 740 Oe | 740 Oe | |
| 740 Oe | 740 Oe | Intrinsic | |
| Magnetic Remanence, Br | 7500 Gauss | 7500 Gauss | |
| Magnetic Maximum Energy Product, BH | 7.5 MGOe | 7.5 MGOe | |
| Curie Temperature | 860 °C | 1580 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Reversible Temp Coef., Bd | -0.02 %/°C | |
| Reversible Temp Coef., Hd | +0.02 %/°C | |
| Temperature Coefficient, Br | -0.025 %/°C | (20-100°C) |
| Temperature Coefficient, Hci | +0.01 %/°C | (20-100°C) |