American Elements Dysprosium Nanoparticles

Category Metal , Nonferrous Metal , Pure Element
Manufacturer American Elements
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF American Elements Dysprosium Nanoparticles.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
General DescriptionDysprosium (Dy) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Dysprosium Particles are typically 10 - 80 nanometers (nm) with specific surface area (SSA) in the 30 – 60 m 2 /g range. Nano Dysprosium Particles are also available in passivated and Ultra high purity and high purity and coated and dispersed forms. Research into applications for dysprosium nanocrystals has focused on use as a dopant in glass and optical fibers, in phosphors, nanophosphors and doped phosphorous nanoparticles and for their potential electrical, dielectric, magnetic, optical, imaging, catalytic, biomedical and bioscience properties and for use in coatings, plastics, nanowire, nanofiber and textiles and in alloy and catalyst applications.
Physical Properties Metric English Comments
Particle Size 0.010 - 0.080 µm
0.010 - 0.080 µm
Specific Surface Area 30 - 60 m²/g
30 - 60 m²/g
Molecular Weight 162.5 g/mol
162.5 g/mol
Descriptive Properties Value Comments
Appearance Black
Stability Moderately reactive in air
Users viewing this material also viewed the following: