ArcelorMittal Complex Phase Steel 1000 Very high strength steel, Cold Rolled Steel

Category Metal , Ferrous Metal , Alloy Steel
Manufacturer ArcelorMittal
Trade Name Complex Phase Steel
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ArcelorMittal Complex Phase Steel 1000 Very high strength steel, Cold Rolled Steel.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Available in the following: uncoated (HCT980C) and electrogalvanized (HCT980C+ZE)Description: The Complex Phase family of steels supplements ArcelorMittal's VHSS (very high strength steel) product range. These steels are cold formed to make lightweight structural elements. A number of automotive parts, such as sills and door reinforcements, have simple shapes and the steel is therefore only slightly deformed. For this reason, ArcelorMittal has added the Complex Phase family of steels to its range. These steels offer high as-delivered yield strength and good bendability and stretch flangeability.Applications: Given their high energy absorption capacity and fatigue strength, these grades are particularly well suited for automotive safety components requiring good impact strength and for suspension system components.Information provided by ArcelorMittal
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 980 - 1200 MPa
142000 - 174000 psi
Tensile Strength, Yield 700 - 850 MPa
102000 - 123000 psi
Elongation at Break >= 8.0 %
>= 8.0 %
L<Sub>0</sub>=80 mm, th<3 mm
Component Elements Properties Metric English Comments
Carbon, C <= 0.18 %
<= 0.18 %
Iron, Fe >= 96.82 %
>= 96.82 %
as balance
Manganese, Mn <= 2.4 %
<= 2.4 %
Silicon, Si <= 0.60 %
<= 0.60 %