Arkema Group Pebax® MV 1041 SN 01 Polyether Block Amide (PEBA) (Dry)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyether Block Amide (PEBA)
Manufacturer Arkema
Trade Name Pebax®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Arkema Group Pebax® MV 1041 SN 01 Polyether Block Amide (PEBA) (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
POLYETHER BLOCK AMIDE (PEBA) hardness 60 shore D breathable (high permeability to H2O vapor,CO2,O2) permanent antistatic grade Applications: breathable films (medical, textile....)ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
Water Absorption 12 %
12 %
Moisture Absorption at Equilibrium 1.0 %
1.0 %
Humidity Absorption
Melt Flow 7.3 g/10 min

@Load 1.00 kg,
Temperature 235 °C
7.3 g/10 min

@Load 2.20 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
Tensile Strength, Yield 17.0 MPa
2470 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Elongation at Yield 26 %
26 %
50 mm/min
Tensile Modulus 0.253 GPa
36.7 ksi
1 mm/min
Charpy Impact Unnotched NB
NB
NB
NB
Low Temp
Charpy Impact, Notched NB
NB
1.14 J/cm²

@Temperature -30.0 °C
5.43 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
Melting Point 170 °C
338 °F
10°C/min
Oxygen Index 22.9 %
22.9 %
Optical Properties Metric English Comments
Transmission, Visible 80 %
80 %
Mfr. reports 'Transparent' but doesn't quantify.
Electrical Properties Metric English Comments
Electrical Resistivity 5.52e+12 ohm-cm
5.52e+12 ohm-cm
Surface Resistance 5.96e+12 ohm
5.96e+12 ohm
Dielectric Strength 43.5 kV/mm
1100 kV/in
Dissipation Factor 0.00048

@Frequency 1e+6 Hz
0.00048

@Frequency 1e+6 Hz
0.00127

@Frequency 100 Hz
0.00127

@Frequency 100 Hz