Ashley Polymers Ashlene® 526LD Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 526LD Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Modified for toughness at low temperatures, injection molding grade.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.11 g/cc
0.0401 lb/in³
ASTM D792
Water Absorption 1.4 %
1.4 %
ASTM D570
Linear Mold Shrinkage 0.016 cm/cm
0.016 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 116
116
ASTM D785
Tensile Strength, Ultimate 68.0 MPa
9860 psi
ATSM D638
Elongation at Break 40 %
40 %
ASTM D638
Flexural Modulus 2.30 GPa
334 ksi
ASTM D790
Izod Impact, Notched 1.92 J/cm
3.60 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 255 °C
491 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 227 °C
441 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C
174 °F
ASTM D648
Flammability, UL94 HB
HB