Ashley Polymers Ashlene® 63M Nylon 66, Mineral Filled

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 63M Nylon 66, Mineral Filled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
A mineral filled Nylon 66 providing superior stiffness and dimensional stability.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 62.0 MPa
8990 psi
ATSM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Flexural Modulus 4.10 GPa
595 ksi
ASTM D790
Izod Impact, Notched 1.17 J/cm
2.19 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 257 °C
495 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 171 °C
340 °F
ASTM D648