Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total PSC 536 Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Heat Resistant Grade
Manufacturer Total Atofina
Trade Name PSC
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PSC 536 Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Polystyrene 536 is a high melt flow; high heat crystal polystyrene. Designed for fast cycle injection molding and for high output, direct injection profile extrusion for foam applications.Information provided by Total Petrochemicals, Inc.
Physical Properties Metric English Comments
Melt Flow 8.5 g/10 min

@Load 5.00 kg,
Temperature 200 °C
8.5 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 44.8 MPa
6500 psi
ASTM D638
Tensile Modulus 2.96 GPa
430 ksi
ASTM D638
Flexural Strength 80.7 MPa
11700 psi
ASTM D790
Flexural Modulus 2.96 GPa
430 ksi
ASTM D790
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 98.9 °C
210 °F
Heat Distortion, Annealed; ASTM D648
Vicat Softening Point 103 °C
218 °F
ASTM D1525