Austin Novel Materials Texalan® 572D Polyether-based TPU

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyether Grade
Manufacturer Austin Novel Materials
Trade Name Texalan®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Austin Novel Materials Texalan® 572D Polyether-based TPU.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech
Physical Properties Metric English Comments
Density 1.16 - 1.20 g/cc
0.0419 - 0.0434 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 69 - 75
69 - 75
ISO 7619
Tensile Strength >= 55.0 MPa
>= 7980 psi
ISO 37
Tensile Stress >= 30.0 MPa

@Strain 100 %
>= 4350 psi

@Strain 100 %
ISO 37
>= 48.0 MPa

@Strain 300 %
>= 6960 psi

@Strain 300 %
ISO 37
Elongation at Yield >= 320 %
>= 320 %
ISO 37
Tear Strength >= 210 kN/m
>= 1200 pli
ISO 34
K Factor (Wear Factor) <= 40
<= 40
[mm<sup>3</sup>]; ISO 4649
Compression Set <= 45 %

@Temperature 70.0 °C
<= 45 %

@Temperature 158 °F
ISO 815