Axiall 14700 Wire & Cable Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 14700 Wire & Cable Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Clear, flexible PVC compound recommended for SPT applications. Maximum service temperature rating of 80°C.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.17 - 1.21 g/cc
1.17 - 1.21 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 68 - 74
68 - 74
delayed; ASTM D-2240
Tensile Strength, Yield 12.93 MPa
1875 psi
ASTM D-638
Elongation at Yield 400 %
400 %
ASTM D-638
100% Modulus 0.00534 GPa
0.775 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -37.0 °C
-34.6 °F
ASTM D-746
Processing Properties Metric English Comments
Melt Temperature 177 °C
350 °F