Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Axiall 38602 Coax & Telecom Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 38602 Coax & Telecom Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
CATV and general purpose jacket with excellent low temperature properties. UL recognized for 720 hour sunlight resistance in all colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.33 - 1.37 g/cc
1.33 - 1.37 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 76 - 82
76 - 82
delayed; ASTM D-2240
83 - 89
83 - 89
ASTM D-2240
Tensile Strength, Yield 15.5 MPa
2250 psi
ASTM D-638
Elongation at Yield 302.4 %
302.4 %
Air Aging: 7 days @ 113°C; 75-mil plaques; UL 1581
360 %
360 %
ASTM D-638
100% Modulus 0.00752 GPa
1.09 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -44.0 °C
-47.2 °F
ASTM D-746
Oxygen Index 23 %
23 %
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 182 °C
360 °F
Users viewing this material also viewed the following: