Michelman® FiberMax® 5000 Water based medium treatment to replace paraffin wax

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Michelman®
Trade Name Fibermax®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® FiberMax® 5000 Water based medium treatment to replace paraffin wax.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Water based medium treatment to replace paraffin waxUsage: FibreMax® 5000 is a new alternative to paraffin wax for treating medium. It is a repulpable, machine ready fiber treatment with the added benefit of water resistance. FibreMax® 5000 should not interfere with gluability. Application data: FibreMax® 5000 can be applied by blade, rod or roll coater.Food Contact Information when manufactured in the USA:FDA: 175.105: Components of adhesivesInformation provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 0.960 - 0.980 g/cc
0.960 - 0.980 g/cc
pH 10 - 12
10 - 12
Brookfield Viscosity <= 35 cP
<= 35 cP
Spindle # 2, rpm 60
Viscosity Measurement 15 - 20
15 - 20
[sec], EZ cup, Cup # 2
Descriptive Properties Value Comments
Appearance Off-white, thin liquid
Solids Type Synthetic