| Category | Polymer , Thermoplastic , Vinyl (PVC) |
| Manufacturer | Axiall |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Axiall 7803 Rigid PVC, Extrusion High Impact Profile.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.32 g/cc | 1.32 g/cc | ASTM D-792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 105 | 105 | ASTM D-785 |
| Hardness, Shore D | 78 | 78 | ASTM D-2240 |
| Tensile Strength, Yield | 36.7 MPa | 5330 psi | ASTM D-638 |
| Tensile Modulus | 2.00 GPa | 290 ksi | ASTM D-638 |
| Flexural Strength | 60.1 MPa | 8710 psi | ASTM D-790 |
| Flexural Modulus | 1.96 GPa | 284 ksi | ASTM D-790 |
| Izod Impact, Notched | 1.39 J/cm @Thickness 6.35 mm, Temperature -40.0 °C |
2.60 ft-lb/in @Thickness 0.250 in, Temperature -40.0 °F |
ASTM D-256 |
| 2.03 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
3.80 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D-256 | |
| 2.14 J/cm @Thickness 6.35 mm, Temperature -28.9 °C |
4.00 ft-lb/in @Thickness 0.250 in, Temperature -20.0 °F |
ASTM D-256 | |
| 3.52 J/cm @Thickness 3.17 mm, Temperature -28.9 °C |
6.60 ft-lb/in @Thickness 0.125 in, Temperature -20.0 °F |
ASTM D-256 | |
| 4.81 J/cm @Thickness 6.35 mm, Temperature -17.8 °C |
9.00 ft-lb/in @Thickness 0.250 in, Temperature 0.000 °F |
ASTM D-256 | |
| 7.21 J/cm @Thickness 6.35 mm, Temperature 0.000 °C |
13.5 ft-lb/in @Thickness 0.250 in, Temperature 32.0 °F |
ASTM D-256 | |
| 7.53 J/cm @Thickness 3.17 mm, Temperature -17.8 °C |
14.1 ft-lb/in @Thickness 0.125 in, Temperature 0.000 °F |
ASTM D-256 | |
| 11.1 J/cm @Thickness 6.35 mm, Temperature 22.8 °C |
20.8 ft-lb/in @Thickness 0.250 in, Temperature 73.0 °F |
ASTM D-256 | |
| 11.6 J/cm @Thickness 3.17 mm, Temperature 0.000 °C |
21.7 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
ASTM D-256 | |
| 13.2 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
24.8 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D-256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 72.0 µm/m-°C @Temperature 20.0 °C |
40.0 µin/in-°F @Temperature 68.0 °F |
ASTM D-696 |
| Deflection Temperature at 1.8 MPa (264 psi) | 66.1 °C | 151 °F | ASTM D-648 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 191 - 196 °C | 375 - 385 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Cell Classification | 16223 | ASTM D-1784 |