Axiall 8843 Moldings & Extrusions Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 8843 Moldings & Extrusions Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
General purpose, non-lead stabilized extrusion compound. Well suited for 80°C rated automotive tubing.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.27 - 1.31 g/cc
1.27 - 1.31 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 80 - 86
80 - 86
delayed; ASTM D-2240
Tensile Strength, Yield 17.6 MPa
2550 psi
ASTM D-638
Elongation at Yield 350 %
350 %
ASTM D-638
100% Modulus 0.00896 GPa
1.30 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -32.0 °C
-25.6 °F
ASTM D-746
Processing Properties Metric English Comments
Melt Temperature 182 °C
360 °F