Material Notes:
Type of Pigment: Azo pigment, Ca/Na Lake Recommendations for food applications: Germany and FranceApplications: LDPE, HDPE/PP, PVC-P, PVC-U, PS, ABSInformation provided by BASF
Physical Properties Metric English Comments
Bulk Density 0.200 g/cc
0.00723 lb/in³
Density 2.80 g/cc
0.101 lb/in³
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 300 °C
572 °F
Descriptive Properties Value Comments
Color Yellow
Migration Fastness 4-5