Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Bapolan® 6403 Polystyrene, Extrusion Grade

Category Polymer , Thermoplastic , Polystyrene (PS)
Manufacturer Bapolan®
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bapolan® 6403 Polystyrene, Extrusion Grade.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Bapolan PS6403 is a high impact polystyrene resin designed for extrusion-thermoforming applications. It complies with US FDA21 CFR177.1640 and 94HB UL rating.Applications: General purpose, housewares, and housing.Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers. All data is based on molded plaques.
Physical Properties Metric English Comments
Melt Flow 3.0 g/10 min
3.0 g/10 min
200C'/5,000g; ASTM D-1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.5 MPa
3550 psi
ASTM D-638
Elongation at Yield 46 %
46 %
ASTM D-638
Flexural Modulus, 1% Secant 2206 MPa
320000 psi
ASTM D-790A
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D-256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °C
199 °F
ASTM D-648
Descriptive Properties Value Comments
Process Extrusion
Region Europe/Turkey
Bamberger Polymers Distribution
International
Bamberger Polymers Distribution
Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved