BecauseWeCare BF90 Biodegradable Plastic

Category Polymer , Renewable/Recycled Polymer , Thermoplastic
Manufacturer BecauseWeCare Pty Ltd.
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF BecauseWeCare BF90 Biodegradable Plastic.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Biodegradable and compostable product produced from corn and developed to break down within weeks in a compost environment, without leaving any harmful residues in the process. Certified to the various worldwide standards of compostability including the Australian Standard AS4736-2006, the European Standard EN13432-2000 and the American Standard ASTM D6400-2004. Good Izod impact strength. Used for bags and film, can be customized for clients.Information provided by BecauseWeCare Pty Ltd.
Physical Properties Metric English Comments
Density 1.15 - 1.20 g/cc
0.0415 - 0.0434 lb/in³
Melt Flow 1.5 - 6.0 g/10 min
<br>@Load 2.16 kg,<br> Temperature 200 °C
1.5 - 6.0 g/10 min
<br>@Load 4.76 lb,<br> Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength 25.0 MPa
3630 psi
100 mm/min; ASTM D638
Elongation at Break 453 %
453 %
100 mm/min; ASTM D638
Processing Properties Metric English Comments
Processing Temperature <= 160 °C
<= 320 °F
Limit
Rear Barrel Temperature 120 - 125 °C
248 - 257 °F
Middle Barrel Temperature 123 - 128 °C
253 - 262 °F
Front Barrel Temperature 115 - 120 °C
239 - 248 °F
Melt Temperature 115 - 120 °C
239 - 248 °F
Mold Temperature 120 - 125 °C
248 - 257 °F
Descriptive Properties Value Comments
Injection Speed Slow to Moderate