Material Notes:
Prisma 3410 is a medium melt flow rate random copolymer designed for injection molding. This product exhibits exceptional transparency, very good stiffness/impact strength balance, and excellent processability. Its applications include: high-transparency parts, household appliances, and high-transparency flip-top lids and packages.
Physical Properties Metric English Comments
Density 0.902 g/cc
0.0326 lb/in³
ASTM-D792
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 230 °C
10 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 82
82
ASTM-D785
Tensile Strength, Yield 29.0 MPa
4210 psi
ASTM-D638
Elongation at Yield 13 %
13 %
ASTM-D638
Flexural Modulus, 1% Secant 1000 MPa
145000 psi
ASTM-D790
Izod Impact, Notched 0.190 J/cm

@Temperature -20.0 °C
0.356 ft-lb/in

@Temperature -4.00 °F
ASTM-D256
0.560 J/cm

@Temperature 23.0 °C
1.05 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C
185 °F
ASTM-D648
Deflection Temperature at 1.8 MPa (264 psi) 51.0 °C
124 °F
ASTM-D648
Vicat Softening Point 129 °C

@Load 1.02 kg
264 °F

@Load 2.25 lb
ASTM-D1525
Optical Properties Metric English Comments
Haze 7.0 %

@Thickness 1.00 mm
7.0 %

@Thickness 0.0394 in
ASTM-D1003