| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Flow |
10
g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C
|
10
g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F
|
STN EN ISO 1133 |
|
Plastcom PLASTALEN® PQ 83 T 30 Polypropylene reinforced with mineral filler
Impact modified PP for injection molding with the content of 30 % mineral filler. Application in automotive industry. Delivered in black grade.Information Provided by Plastcom spol. s r.o.
|
|||
| Melt Flow |
10
g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C
|
10
g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F
|
Procedure A Condition L; ASTM D1238 |
|
Network Polymers PC-1010
Description: Polycarbonate, 10% Glass Filled BlackInformation provided by Network Polymers Inc.
|
|||
| Melt Flow |
10
g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C
|
10
g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F
|
ASTM D1238 |
|
SABIC Innovative Plastics Lexan® EXL1330 PC Copolymer (Asia Pacific)
Lexan* EXL1330 polycarbonate (PC) siloxane copolymer resin is a UV stabilized opaque injection molding (IM) and sheet extrusion grade. This resin offers extreme low temperature (-60 C) ductility in ..
|
|||
| Melt Flow |
10
g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C
|
10
g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F
|
ASTM D1238 |
|
SABIC Innovative Plastics Lexan® HPX4EU PC Copolymer (Europe-Africa-Middle East)
Medium flow specialty polycarbonate - improved processability & autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP..
|
|||
| Melt Flow |
10
g/10 min <br>@Load 2.16 kg,<br> Temperature 400 °C
|
10
g/10 min <br>@Load 4.76 lb,<br> Temperature 752 °F
|
ASTM D1238 |
|
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK)
(Unverified Data**)
KetaSpire KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and pro..
|
|||
| Melt Flow |
10
g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C
|
10
g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F
|
ASTM D1238 |
|
SABIC Innovative Plastics Lexan® EXL9330 PC Copolymer
Opaque PC-Siloxane copolymer with excellent processability. Non-chlorinated, non-brominated flame retardant product in most colors. UV-stabilized. UL rated f1/V-0/5VA.
|
|||
| Melt Flow |
10
g/10 min <br>@Load 2.16 kg,<br> Temperature 190 °C
|
10
g/10 min <br>@Load 4.76 lb,<br> Temperature 374 °F
|
ASTM D1238 |
|
NOVA Chemicals Novapol® LM-1019-A LDPE Masterbatch Resin
(discontinued **)
Features: easy processing, good dispersion.Applications: masterbatch/compounding.Data provided by the manufacturer.
|
|||
| Melt Flow |
10
g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C
|
10
g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F
|
ASTM D1238 |
|
Reliance Industries Repol T100MK Polypropylene
REPOL Polypropylene T100MK is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific cataly..
|
|||
| Melt Flow |
10
g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C
|
10
g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F
|
ASTM D1238 |
|
LG Chemical LUPOL ED1045D TPO, Thermoplastic Elastomer
Description: Injection Molding, TPO, Thermoplastic Elastomer, Soft TouchApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0, 1333-86-4, 25087-34-7 and 14807-96-6Information provided..
|
|||
| Melt Flow |
10
g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C
|
10
g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F
|
ASTM D1238 |
|
LG Chemical LUPOL HI5205 PP+MF20%, High Impact
Description: Injection Molding, PP+MF20%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 26221-73-8 and 14807-96-6Information provided by LG Chemical
|
|||
| Melt Flow |
10
g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C
|
10
g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F
|
L; ASTM D1238 |
|
Global CPP-110 10% CaC03 Filled Polypropylene
Information provided by Global Polymers Corporation.
|
|||
| Melt Flow |
10
-
16
g/10 min <br>@Load 2.16 kg,<br> Temperature 250 °C
|
10
-
16
g/10 min <br>@Load 4.76 lb,<br> Temperature 482 °F
|
ASTM D1238 |
|
GRECO ISOPAK 625 Polycarbonate/ABS Alloy
General purpose polycarbonate/ABS alloy; good impact and dimensional stabilityInformation provided by Greater Eastern Resins Industrial Co., Ltd.
|
|||
| Melt Flow |
10
-
13
g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C
|
10
-
13
g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F
|
ASTM D1238 |
|
LTL Color Compounds ColorRxâ„¢ PC-1002AF Food Grade Polycarbonate
A biocompatible, 10 melt grade of Polycarbonate for healthcare applications, containing antimicrobial protection.All information provided by LTL Color Compounders, Inc.
|
|||
| Melt Flow | 10 g/10 min | 10 g/10 min | ISO 1133 |
|
Lucite International Diakon® CLG960 Acrylic Polymer
Information provided by Lucite International
|
|||
| Melt Flow |
10
g/10 min <br>@Load 5.00 kg,<br> Temperature 200 °C
|
10
g/10 min <br>@Load 11.0 lb,<br> Temperature 392 °F
|
ASTM D1238 |
|
Kingfa FRHIPS-722 Flame Retardant Polystyrene
Features:UL 94 V-0 @ 3.2mmHalogen free flame retardantExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV and audio housingElectrical appliance housing..
|
|||
| Melt Flow |
10
g/10 min <br>@Load 21.6 kg
|
10
g/10 min <br>@Load 47.6 lb
|
|
|
Lubrizol Advanced Materials Pearlcoat® Activa D198K Thermoplastic Polyurethane Elastomer
PEARLCOAT® Activa D198K is an aliphatic based thermoplastic polyurethane of low hardness, supplied in form of natural pellets. This product gives an inherent “low gloss aspect†on the f..
|
|||
| Melt Flow |
10
g/10 min <br>@Load 2.16 kg,<br> Temperature 400 °C
|
10
g/10 min <br>@Load 4.76 lb,<br> Temperature 752 °F
|
ASTM D1238 |
|
Solvay Specialty Polymers KetaSpire® KT-850 Polyetheretherketone (PEEK)
KetaSpire® KT-850 is the intermediate-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color pellet form. KetaSpire® PEEK is produced to the highest industry standa..
|
|||
| Melt Flow |
10
g/10 min <br>@Load 2.16 kg,<br> Temperature 400 °C
|
10
g/10 min <br>@Load 4.76 lb,<br> Temperature 752 °F
|
ASTM D1238 |
|
Solvay Specialty Polymers KetaSpire® KT-850P Polyetheretherketone (PEEK)
KetaSpire® KT-850P is the intermediate-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color coarse powder form. KetaSpire® PEEK is produced to the highest industr..
|
|||
| Melt Flow | 10 g/10 min | 10 g/10 min | ASTM D1238 |
|
SPS Guang Zhou POPTREEâ„¢ 6001A Flame-retarded Polyethylene
Characteristic: Low density, medium melt flow index, medium notched impact strength, no bloomingApplications: E/E partsInformation Provided by SPS (Guang Zhou) Ltd.
|
|||
| Melt Flow |
10
g/10 min <br>@Load 5.00 kg,<br> Temperature 260 °C
|
10
g/10 min <br>@Load 11.0 lb,<br> Temperature 500 °F
|
ASTM D1238 |
|
Star Plastics PC/ABSQX7004 Molding Grade PC/ABS
Information provided by Star Plastics, Inc.
|
|||
| Melt Flow |
10
g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C
|
10
g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F
|
ASTM D1238 |
|
Samyang Trirex® 3025PJ Polycarbonate
PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3025PJ is a general use grade.Information provided by Samyang.
|
|||
| Melt Flow |
10
g/10 min <br>@Load 5.00 kg,<br> Temperature 300 °C
|
10
g/10 min <br>@Load 11.0 lb,<br> Temperature 572 °F
|
ASTM D1238 |
|
SABIC Innovative Plastics NORYL GFN1630V PPE+HIPS (Europe-Africa-Middle East)
Noryl* GFN1630V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en..
|
|||
| Melt Flow | 10 g/10 min | 10 g/10 min | ASTM D1238 |
|
A. Schulman POLYFORT™ FPP1666 Talc Filled Homopolymer Polypropylene
DescriptionPolyfort® FPP 1666 is a 10% talc filled homopolymer polypropylene compound. Information provided by A. Schulman.
|
|||
| Melt Flow |
10
g/10 min <br>@Load 2.16 kg,<br> Temperature 190 °C
|
10
g/10 min <br>@Load 4.76 lb,<br> Temperature 374 °F
|
ASTM D1238 |
|
Westlake EC4042AA Low Density Polyethylene
WESTLAKE low-density polyethylene EC4042 is a low density resin designed for applications, such as sugar pouches and freezer wrap, where high coating speeds and good drawdown are required. The combi..
|
|||
| Melt Flow |
10
g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C
|
10
g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F
|
ASTM D1238 |
|
ExxonMobil AP3AW Polypropylene Impact Copolymer
Product Description: A UV stabilized medium impact copolymer resin designed for automotive battery cases.Availability: Asia Pacific Features:Good UV ResistanceHigh StiffnessLow WarpageMedium FlowMe..
|
|||
| Melt Flow | 10 - 16 g/10 min | 10 - 16 g/10 min | ASTM D1238 |
|
Buckeye Polymers BP RPP 4010 T NAT Polypropylene, Talc Filled
Product Information: Our Talc filled product lines exhibit excellent properties such as high stiffness, surface aesthetics, low coefficient of thermal expansion, low shrinkage, improved scratch and ..
|
|||
| Melt Flow | 10 g/10 min | 10 g/10 min | ASTM D-1238 |
|
Bapolene® 3257U Polyethylene, Injection Molding
Bapolene 3257U is a high density polyethylene resin that offers improved cycle times, superior modulus and impact resistance. It complies with US FDA 21CFR177.1520 and has a UV protection package.A..
|
|||
| Melt Flow |
10
g/10 min <br>@Load 21.6 kg,<br> Temperature 185 - 195 °C
|
10
g/10 min <br>@Load 47.6 lb,<br> Temperature 365 - 383 °F
|
|
|
Lubrizol Advanced Materials Pearlthane® ECO D20N88 Thermoplastic Polyurethane
(discontinued **)
PEARLTHANE® ECO D20N88 is a 86 Shore A, High Performance natural TPU based on Renewable Sources with ca. 60% renewable content according to ASTM D6866 for Extrusion and Injection Molding applicatio..
|
|||
| Melt Flow |
10
g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C
|
10
g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F
|
ASTM D1238 |
|
SABIC Innovative Plastics Lexan® HP4EU PC (Europe-Africa-Middle East)
Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mold ..
|
|||