Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

CPC - Vycom SEABOARD™ LITE High density polyethylene (HDPE)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer CPC - Vycom Co.
Trade Name SEABOARD™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CPC - Vycom SEABOARD™ LITE High density polyethylene (HDPE).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Seaboard Lite is a high density polyethylene (HDPE) sheet formulated to meet the specific requirements of marine and other outdoor environments. Seaboard Lite is UV stable and will withstand the elements without rotting, delaminating or peeling like wood. CPC Seaboard Lite is manufactured as a continuous extrusion. It is not press laminated. Thus, it is unconditionally guaranteed not to delaminate during the service life of the end-product.FEATURES AND BENEFITS Inert- Seaboard Lite is inert in marine environments and is not effected by moisture and most cleaning chemicals. Toughness- Seaboard Lite is made from the same tough high density polyethylene (HDPE) as our standard grade of Seaboard. Moisture resistance- Seaboard Lite is resistant to moisture and it will not rot or swell in moist environments. Light- Seaboard Lite is 30% lighter than standard high density polyethylene (HDPE).Information provided by Compression Polymers Corp - Vycom
Physical Properties Metric English Comments
Density 0.800 g/cc
0.0289 lb/in³
ASTM D1505
Environmental Stress Crack Resistance 25 hour
25 hour
F50; ASTM D1693
>= 500 hour
>= 500 hour
F50; ASTM D2561
Mechanical Properties Metric English Comments
Hardness, Shore D 69
69
ASTM D2240
Tensile Strength, Ultimate 22.1 MPa
3200 psi
ASTM D638
Flexural Strength 27.6 MPa
4000 psi
ASTM D790
Flexural Modulus 1.57 GPa
228 ksi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 50.0 °C
122 °F
ASTM D648
Vicat Softening Point 129 °C
264 °F
ASTM D1525
Brittleness Temperature -76.1 °C
-105 °F
ASTM D746