Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

California Fine Wire Alloy 406 Precious Metal Alloy

Category Metal , Nonferrous Metal
Manufacturer California Fine Wire
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF California Fine Wire Alloy 406 Precious Metal Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
All values may vary dependent on specific design and usageProprietary compositionCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Physical Properties Metric English Comments
Density 10.9 g/cc
0.395 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 524 MPa
76000 psi
Stress relieved
586 MPa
85000 psi
Hard
Modulus of Elasticity 47.0 GPa
6820 ksi
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000125 ohm-cm
0.0000125 ohm-cm
3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02
Descriptive Properties Value Comments
Magnetic None
Temperature Coefficient of Resistance 0.0004 ohms/ohm-°C
0-100°C
Thermal EMF vs. Copper -0.055 mV
Users viewing this material also viewed the following: