Carborundum CarboTherm™ CTL30 Boron Nitride Powder

Category Ceramic , Nitride , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Carborundum
Trade Name CarboTherm™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Carborundum CarboTherm™ CTL30 Boron Nitride Powder.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Boron Nitride powders have high thermal conductivity, low dielectric loss, and low thermal expansion. They are non-abrading to electronic components, lubricious, non-toxic, and retain their dielectric properties at elevated temperatures. Applications include: use in potting compounds, encapsulants, epoxies, silicone oils and resins, and thermoplastics; use as a processing aid; use as a nucleating and foaming agent. Carborundum's CarboTherm™ powders can be custom blended to yield specific properties. Particle size and distribution can be tailored to give optimum fill and flowability while still maintaining high purity and consistency. CTL30 particles are platelets. Data provided by the manufacturer, Carborundum Corporation.
Physical Properties Metric English Comments
Apparent Bulk Density 0.600 g/cc
0.0217 lb/in³
Tap density
Particle Size 7.0 - 11 µm
7.0 - 11 µm
Mean
Component Elements Properties Metric English Comments
B2O3 0.40 %
0.40 %
BN 99.4 %
99.4 %
O2 0.70 %
0.70 %
includes the oxygen in B2O3