Category Metal , Ferrous Metal , Alloy Steel , Tool Steel
Manufacturer Carpenter Technology Corporation (Cartech)
Trade Name AerMet®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Carpenter AerMet® 340.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Physical Properties Metric English Comments
Density 7.86 g/cc
0.284 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 2430 MPa
352000 psi
Tensile Strength, Yield 2160 MPa
314000 psi
Elongation at Break 11.3 %
11.3 %
Reduction of Area 55.2 %
55.2 %
Tensile Modulus 192 GPa
27900 ksi
Fatigue Strength 986 MPa

@# of Cycles 1.00e+7
143000 psi

@# of Cycles 1.00e+7
R=-1, Kt=1
Fracture Toughness 34.61 MPa-m½
31.50 ksi-in½
Charpy Impact 14.6 J
10.8 ft-lb
notched