Micro-Melt® 10 tool steel is a high vanadium tool steel produced using the Carpenter Micro-Melt powder process. This grade possesses wear resistance superior to most other tool steels along with good strength and toughness characteristics. Many of the benefits realized in the use of Micro-Melt powder metals, such as Micro-Melt® 10 alloy, are a direct result of the refined microstructure (smaller, more uniformly distributed carbide particles and a finer grain size) and the lack of segregation in the powder metallurgy product. These advantages include ease of grinding, improved response to heat treatment, greater wear resistance, and increased toughness of the finished tool. Micro-Melt 10 tool steel changes size only slightly after hardening. An expansion of about 0.0004 inches/inch is typical.Applications: punches, dies for blanking, piercing dies, forming rolls and dies, cold heading, steel mill rolls, cold extrusion, slitter knives, shears, pelletizer blades, nozzles, woodworking tools, cold extrusion barrels, cold extrusion liners, plastic injection molds, compacting toolsInformation provided by Carpenter Technology Corporation.Micro-Melt® is a registered trademark of Carpenter Technology Corporation.
Physical Properties Metric English Comments
Specific Gravity 7.45 g/cc
7.45 g/cc
Mechanical Properties Metric English Comments
Hardness, Rockwell C 63
63
Modulus of Elasticity 200 GPa
29000 ksi
Izod Impact Unnotched 29.8 J
22.0 ft-lb
Abrasion 9.0
9.0
loss in mm<sup>3</sup>, after 30 minutes; ASTM G65
Thermal Properties Metric English Comments
CTE, linear 10.72 µm/m-°C

@Temperature 21.0 - 100 °C
5.956 µin/in-°F

@Temperature 69.8 - 212 °F
11.13 µm/m-°C

@Temperature 21.0 - 260 °C
6.183 µin/in-°F

@Temperature 69.8 - 500 °F
12.32 µm/m-°C

@Temperature 21.0 - 538 °C
6.844 µin/in-°F

@Temperature 69.8 - 1000 °F
Component Elements Properties Metric English Comments
Carbon, C 2.4 - 2.5 %
2.4 - 2.5 %
Chromium, Cr 4.75 - 5.75 %
4.75 - 5.75 %
Iron, Fe 78.21 - 81.35 %
78.21 - 81.35 %
As Balance
Manganese, Mn 0.35 - 0.60 %
0.35 - 0.60 %
Molybdenum, Mo 1.1 - 1.5 %
1.1 - 1.5 %
Silicon, Si 0.75 - 1.1 %
0.75 - 1.1 %
Sulfur, S 0.050 - 0.090 %
0.050 - 0.090 %
Vanadium, V 9.25 - 10.25 %
9.25 - 10.25 %