Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chase Plastics CP Pryme® NN200STL (DAM) Nylon 66, Super-Toughened, Internally Lubricated

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Impact Grade
Manufacturer Chase Plastics
Trade Name CP Pryme®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chase Plastics CP Pryme® NN200STL (DAM) Nylon 66, Super-Toughened, Internally Lubricated.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Chase Plastics.
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 42.1 MPa
6100 psi
ASTM D638
Elongation at Break 90 %
90 %
ASTM D638
Flexural Strength 57.2 MPa
8300 psi
ASTM D790
Flexural Modulus 1.38 GPa
200 ksi
ASTM D790
Izod Impact, Notched 8.54 J/cm
16.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 54.4 °C
130 °F
ASTM D648