Mechanical Properties Metric English Comments
Flexural Modulus 1.38 GPa
200 ksi
Tangent; ASTM D790
RheTech Products HP521-231 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 173B Navy Blue
Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus >= 1.38 GPa
>= 200 ksi
ASTM D790
S&E Specialty Polymers GPP™ 1005M-EXLT PP
Application: UL94 V-2, Non-blooming flame retardant polypropylene compound for injection molding.Information provided by S&E Specialty Polymers
Flexural Modulus 1.38 GPa
200 ksi
ASTM D790
S&E Specialty Polymers TufGuard M™ GPP1001M-P-2986 Grey PP, Flame Retardant
Application: High impact resistant, non-blooming flame retardant polypropylene compound designed for UL94 V-0 injection molding applications.Information provided by S&E Specialty Polymers
Flexural Modulus 1.38 GPa
200 ksi
Tangent; ASTM D790
RheTech Products HP522-473 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, ZU5A Dark Graphite
Applications: ConsolesClose out panelInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 1.38 GPa
200 ksi
ASTM D790
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 5% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Flexural Modulus 1.38 GPa
200 ksi
Tangent; ASTM D790
Flint Hills AP5325-HS Impact Copolymer Polypropylene
High impact copolymer, UL certified, and FDA compliant. Features: Nucleated and heat stabilizedApplications: Injection molding: large, thin wall automotive interior parts.Former Huntsman polypropyle..
Flexural Modulus 1.38 GPa
200 ksi
1% Secant, 0.05 in/min; ASTM D790
LyondellBasell Pro-faxâ„¢ PH350 Polypropylene Homopolymer
Description: Pro-faxâ„¢ PH350 general purpose polypropylene homopolymer resin is available as natural flake. Flake form resin is well suited for mixing with pigments and other additives to make p..
Flexural Modulus 1.38 GPa
200 ksi
tangent; ASTM D790
Spartech PP7110 Talc Filled High Impact Copolymer
Good material choice for applications where low to medium levels of impact are required and where stiffness and heat deflection properties remain criticalInformation provided by Spartech
Flexural Modulus 1.38 GPa
200 ksi
ASTM D790
Techmer ES Statiblend® POM CO AS BK
Availability: North AmericaForms: PelletsAdditive: AntistaticFeature: Antistatic and ConductiveAppearance: BlackInformation provided by TP Composites, Inc.
Flexural Modulus 1.38 GPa
200 ksi
ASTM D790
ScanTube ETFE Tubing
Information provided by ScanTube, Inc.
Flexural Modulus 1.38 GPa
200 ksi
1.3 mm/min; ASTM D790
A. Schulman POLYPUR™ FPU 1380 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Flexural Modulus 1.38 GPa
200 ksi
ASTM D790
A. Schulman PP 3488-01 Polypropylene Homopolymer Polypropylene
DescriptionPolypropylene PP 3488-01 is a specially formulated homopolymer polypropylene designed for large appliance injection molding. This material has excellent chemical resistance in addition t..
Flexural Modulus 1.38 GPa
200 ksi
ASTM D790
A. Schulman PP 3488-01 Polypropylene Homopolymer Polypropylene
DescriptionPolypropylene PP 3488-01 is a specially formulated homopolymer polypropylene designed for large appliance injection molding. This material has excellent chemical resistance in addition t..
Flexural Modulus 1.38 GPa
200 ksi
ASTM D 790
Total 5502 BZ HDPE injection blow molding
Applications: Cosmetics and toiletries, pharmaceuticals, specialty containers, food packagingInformation provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atof..
Flexural Modulus 1.38 GPa
200 ksi
1.3mm per min, 1% secant; ASTM D790
Formosa Plastics Formolene® 2306N Impact Copolymer Polypropylene
Impact Copolymer for Compression and Injection Molded Caps and Closures Formolene® 2306N is a polypropylene copolymer formulated for compression and injection molded cap applications. It was create..
Flexural Modulus 1.38 GPa
200 ksi
1.3mm per min, 1% secant; ASTM D790
Formosa Plastics Formolene® 5144H Homopolymer Polypropylene
Homopolymer for Appliance Applications Formolene® 5144H is a highly isotactic polypropylene homopolymer designed for consumer products and appliance applications requiring long-term heat-aging res..
Flexural Modulus 1.38 GPa
200 ksi
ASTM D790
Formosa Plastics Formolene® HB5502S1 Sheet and Thermoforming HDPE
High Density Polyethylene Hexene CopolymerApplications: Molded or formed industrial housings and parts, tanks, shrouds.Formolene HB5502S1 HDPE resin is designed for applications requiring excellent ..
Flexural Modulus 1.38 GPa
200 ksi
1.3 mm/min; ASTM D790
A. Schulman POLYPUR™ FPU 1380 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Flexural Modulus 1.38 GPa
200 ksi
ASTM D790
A. Schulman PP 3490-01G Polypropylene Homopolymer Polypropylene
DescriptionPolypropylene PP 3490-01G Natural is a homopolymer for extrusion and compounding applications. This material can also be used as a carrier resin for color concentrates. ApplicationPP 349..
Flexural Modulus 1.38 GPa
200 ksi
ASTM D790
Formosa Plastics Formolene® HB5502B Blow Molding HDPE
Hexene CopolymerApplications: Injection blow molded pharmaceutical packagingFormolene HB5502B is designed for applications requiring excellent stiffness and stress crack resistance properties. It ma..
Flexural Modulus 1.38 GPa
200 ksi
CMW® ELKONITE® 10W53 Heat Treatable Copper Tungsten
Uses: Resistance / projection welding electrodesInformation provided by CMW Inc.
Flexural Modulus 1.38 GPa
200 ksi
0.05 in/min, 1% secant; ASTM D-790A
Braskem FPT300F Homopolymer Polypropylene
Description: Good mold release, excellent part finish (low bloom).Applications: Suggested uses include housewares, caps and closures, mugs / cups, thin-walled containers.Process: Injection Molding.T..
Flexural Modulus 1.38 GPa
200 ksi
0.05 in/min; 1% secant; Procedure A; ASTM D790
Phillips 66 COPYLENE® CH014 Polypropylene, Homopolymer, Extrusion, Strapping
COPYLENE™ CH014 is a polypropylene homopolymer resin designed for extrusion applications. Applications: Raffia/Tapes/Strapping; Geotextile & Agriculture; Nets. Equivalent to Pro-fax® HL781GInforma..
Flexural Modulus 1.38 GPa
200 ksi
0.05 in/min; 1% secant; Procedure A; ASTM D790
Phillips 66 COPYLENE® CH016 Polypropylene, Homopolymer, BOPP
COPYLENE™ CH016 is a polypropylene homopolymer resin designed for BOPP (biaxially oriented polypropylene) film extrusion applications. Applications: Bags & Pouches; Raffia/Tapes/Strapping; Peelable..
Flexural Modulus 1.38 GPa
200 ksi
1.3 mm/min; ASTM D790
A. Schulman POLYPUR™ FPU 1380 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Flexural Modulus 1.38 GPa
200 ksi
1.3mm per min, 1% secant; ASTM D790
Formosa Plastics Formolene® 1102K Cast and BOPP Film Polypropylene
HomopolymerApplications: Biaxially oriented film.Formolene 1102K is a high molecular weight, highly isotactic polypropylene homopolymer designed for extrusion processes, notably biaxially oriented f..
Flexural Modulus 1.38 GPa

@Temperature 23.0 °C
200 ksi

@Temperature 73.4 °F
ASTM D790A
Ineos H35G-00 Polypropylene Homopolymer
This is a general purpose homopolymer for injection molding applications. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.ApplicationsC..
Copyright © lookpolymers.com All Rights Reserved