Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Cheng Yu Plastic FR200GV10 Flame Retardant Nylon 66, 10% Glass Fiber

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass Fiber Filled, Flame Retardant
Manufacturer Cheng Yu Plastic Company Limited (formerly Luen Cheong Hong)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cheng Yu Plastic FR200GV10 Flame Retardant Nylon 66, 10% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
ASTM D792
Water Absorption 1.0 - 2.0 %
1.0 - 2.0 %
ASTM D570
Linear Mold Shrinkage 0.0020 - 0.020 cm/cm
0.0020 - 0.020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 95
95
ASTM D785
Tensile Strength, Yield 98.1 MPa
14200 psi
ASTM D638
Flexural Yield Strength 132 MPa
19200 psi
ASTM D790
Izod Impact, Notched 0.735 J/cm
1.38 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 245 °C
473 °F
ASTM D648
Flammability, UL94 V-0
V-0