Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Cheng Yu Plastic N6GV20 Flame Retardant Nylon 6, 20% Glass Filled

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 20% Glass Fiber Filled
Manufacturer Cheng Yu Plastic Company Limited (formerly Luen Cheong Hong)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cheng Yu Plastic N6GV20 Flame Retardant Nylon 6, 20% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Water Absorption 0.15 %
0.15 %
ASTM D570
Linear Mold Shrinkage 0.0080 - 0.015 cm/cm
0.0080 - 0.015 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 94
94
ASTM D785
Tensile Strength, Yield 142 MPa
20600 psi
ASTM D638
Flexural Yield Strength 230 MPa
33400 psi
ASTM D790
Izod Impact, Notched 0.902 J/cm
1.69 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 228 °C
442 °F
ASTM D648
Flammability, UL94 V-0
V-0