Material Notes:
Metallocene linear low density polyethylene. This linear low density, hexene copolymer is tailored for blow molded containers that require: High glossGood clarityExcellent ESCR Applications: Typical blow molded applications for C101 include: Glossy multilayer bottlesSqueezable bottlesInformation provided by PhillipsThis resin meets these specifications: ASTM D4976 - PE 213FDA 21 CFR 177.1520(c) 3.2a, use conditions B through H per 21 CFR 176.170(c)
Physical Properties Metric English Comments
Density 0.916 g/cc
0.0331 lb/in³
ASTM D-1505
ESCR 100% Igepal® >= 1000 hour
>= 1000 hour
Condition A, F50; ASTM D-1693
>= 1000 hour
>= 1000 hour
Condition B, F50; ASTM D-1693
Melt Index of Compound 1.4 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.4 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D-1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 10.0 MPa
1450 psi
2 in/min, Type IV bar; ASTM D-638
Elongation at Break 600 %
600 %
2 in/min, Type IV bar; ASTM D-638
Flexural Modulus 0.270 GPa
39.2 ksi
Tangent - 16:1 span:depth, 0.5 in/min; ASTM D-790
Thermal Properties Metric English Comments
Brittleness Temperature <= -75.0 °C
<= -103 °F
Type A, Type I specimen; ASTM D-746