Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chevron Phillips Marlex® HXM 50100-01 Extra high molecular weight hexene copolymer

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), UHMW PE Ultra High Molecular Weight
Manufacturer Chevron Phillips Chemical Company LP
Trade Name Marlex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips Marlex® HXM 50100-01 Extra high molecular weight hexene copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Benefits: excellent balance of stress cracking resistance, good melt strength, excellent stress cracking resistance, good rigidity, excellent impact strength even at low temperaturesApplications: 55-gallon shipping containers, gasoline tanks, agricultural chemical tanks, pallets, cattle feeders, large formed parts, boatsInformation provided by Chevron Phillips Chemical Company
Physical Properties Metric English Comments
Density 0.949 g/cc
0.0343 lb/in³
ASTM D1505
Environmental Stress Crack Resistance >= 600 hour

@Temperature 50.0 °C
>= 600 hour

@Temperature 122 °F
Condition A and Condition B; ASTM D 1693
High Load Melt Index 12 g/10 min

@Load 21.6 kg,
Temperature 190 °C
12 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.0 MPa
3630 psi
ASTM D638 Type IV
Elongation at Break >= 600 %
>= 600 %
ASTM D638 Type IV
Flexural Modulus 1.20 GPa
174 ksi
ASTM D790
Thermal Properties Metric English Comments
Brittleness Temperature <= -91.0 °C
<= -132 °F
ASTM D746
Processing Properties Metric English Comments
Processing Temperature 154 - 182 °C
309 - 360 °F
Thermoforming Surface
188 - 232 °C
370 - 450 °F
Blow Molding
232 - 268 °C
450 - 514 °F
Extrusion
Users viewing this material also viewed the following: