China Tungsten Kmo51-A Molybdenum Concentrate

Category Metal , Nonferrous Metal , Molybdenum Alloy
Manufacturer China Tungsten
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF China Tungsten Kmo51-A Molybdenum Concentrate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by China Tungsten
Component Elements Properties Metric English Comments
Arsenic, As <= 0.020 %
<= 0.020 %
Bismuth, Bi <= 0.060 %
<= 0.060 %
CaO <= 1.8 %
<= 1.8 %
Copper, Cu <= 0.20 %
<= 0.20 %
Lead, Pb <= 0.18 %
<= 0.18 %
Molybdenum, Mo >= 51 %
>= 51 %
Phosphorous, P <= 0.020 %
<= 0.020 %
Potassium, K <= 38.64 %
<= 38.64 %
SiO2 <= 8.0 %
<= 8.0 %
Tin, Sn <= 0.020 %
<= 0.020 %
Descriptive Properties Value Comments
Tungsten Trioxide, WO3 (%), max 0.06