Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0050 - 0.0060 cm/cm
0.0050 - 0.0060 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 38.6 MPa
5600 psi
ASTM D638
Elongation at Break 40 %
40 %
ASTM D638
Flexural Modulus 2.24 GPa
325 ksi
ASTM D790
Izod Impact, Notched 2.67 J/cm
5.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 88.9 °C
192 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 76.7 °C
170 °F
ASTM D648