ConocoPhillips Centak Centak 11 Extreme Pressure Gear Lubricant

Category Fluid , Lubricant , Calcium Gellant , Organic Soap Gellant
Manufacturer ConocoPhillips
Trade Name Centak
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ConocoPhillips Centak Centak 11 Extreme Pressure Gear Lubricant.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Conoco Centak is a high-quality, multipurpose, extreme-pressure gear lubricant recommended for the open gears of shovels and draglines. It may also be used in grinding mills, swing gears and pinions, dipper sticks, rails and rollers, as well as plain and lowspeed roller bearings. Centak 11 is an NLGI No. 1 grade, providing flexibility in application over a wide temperature range. The product is smooth, black and viscous semifluid. Centak 11 also has good pumpability and is recommended for automated lubrication systems. Centak is manufactured with a calcium soap and a high-viscosity base oil. It also contains polymers, resins and solid lubricants. However, Centak contains no heavy metals, solvents or asphaltic material.Information provided by ConocoPhillips.
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 735 cSt
735 cSt
Base Oil Viscosity
Kinematic Viscosity at 100°C (212°F) 33.4 cSt
33.4 cSt
Base Oil Viscosity
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Load Wear Index 60
60
Four Ball Extreme Pressure, Weld Load 500 kg
1100 lb (mass)
Weld Load
Four Ball Wear 0.400 mm
0.0157 in
Penetration P(60), 1/10 mm 320
320
Timken Test 34000 g
75.0 lb
Thermal Properties Metric English Comments
Pour Point 0.000 °C
32.0 °F
Flash Point 321 °C
610 °F
Dropping Point 132 °C
270 °F
Descriptive Properties Value Comments
Color Black
Soap Type (Thickener) Calcium
Texture Smooth