Covestro Bayfol® CR 1-4 Polycarbonate + PBT

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer Covestro
Trade Name Bayfol®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Covestro Bayfol® CR 1-4 Polycarbonate + PBT.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Bayfol CR 1-4 is an extruded film based on a Makrolon(PC)/Pocan(PBT)-blend comprising high dynamic strength, good cold formability and increased chemical resistance. The color is translucent nature, the surface combination is one side gloss - one side fine matte. It is available in various standard thicknesses between 125 - 250 micron. Other thicknesses on requestAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Descriptive Properties Value Comments
Availability Europe
Near East/Africa
North America
South and Central America