Material Notes:
High Performance FR. Properties for dry as molded samples.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 65.0 MPa
9430 psi
ASTM D638
Flexural Yield Strength 90.0 MPa
13100 psi
ASTM D790
Flexural Modulus 2.40 GPa
348 ksi
ASTM D790
Izod Impact, Notched 2.50 J/cm
4.68 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 127 °C
261 °F
ASTM D648