Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Cytec Thornel® Mat VME Carbon Fiber

Category Carbon , Carbon Fiber , Other Engineering Material , Composite Fibers
Manufacturer Cytec
Trade Name Thornel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cytec Thornel® Mat VME Carbon Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Data provided by the manufacturer, Amoco Performance Products, Inc.Form of mat VMA with shorter fibers for injection molding. Fiber lengths average 200 µm - inadequate for good mechanical property improvement but can result in improved shrinkage, thermal and electrical conductivity, and frictional characteristics.98% carbon assay, 13 µm filament diameterThornel® products were sold by Amoco and are now owned by Cytec.
Physical Properties Metric English Comments
Density 2.00 g/cc
0.0723 lb/in³
Filament Property.
Apparent Bulk Density 0.600 g/cc
0.0217 lb/in³
Specific Surface Area 0.40 m²/g
0.40 m²/g
Filament Property
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1400 MPa
203000 psi
Filament Property. Mat strength is 120 N/m
Modulus of Elasticity 170 GPa
24700 ksi
Filament property, in tension
Thermal Properties Metric English Comments
Thermal Conductivity 0.410 W/m-K
2.85 BTU-in/hr-ft²-°F
across thickness of mat
Electrical Properties Metric English Comments
Electrical Resistivity 0.00120 ohm-cm
0.00120 ohm-cm
Filament
0.700 ohm-cm
0.700 ohm-cm
Mat