Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DSM Novamid® 2330J PA666

Category Polymer , Thermoplastic , Nylon , Nylon 6/66
Manufacturer DSM Engineering Plastics
Trade Name Novamid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Novamid® 2330J PA666.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Film Extrusion, Extrusion, Extrusion Grade
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
dry; ISO 1183
Moisture Absorption 3.50 %
3.50 %
Sim. To ISO 62
Viscosity 90000 cP

@Shear Rate 10000 1/s,
Temperature 240 °C
90000 cP

@Shear Rate 10000 1/s,
Temperature 464 °F
90000 cP

@Shear Rate 10000 1/s,
Temperature 260 °C
90000 cP

@Shear Rate 10000 1/s,
Temperature 500 °F
90000 cP

@Shear Rate 10000 1/s,
Temperature 280 °C
90000 cP

@Shear Rate 10000 1/s,
Temperature 536 °F
2.00e+6 cP

@Shear Rate 0.100 1/s,
Temperature 280 °C
2.00e+6 cP

@Shear Rate 0.100 1/s,
Temperature 536 °F
3.00e+6 cP

@Shear Rate 0.100 1/s,
Temperature 260 °C
3.00e+6 cP

@Shear Rate 0.100 1/s,
Temperature 500 °F
4.50e+6 cP

@Shear Rate 0.100 1/s,
Temperature 240 °C
4.50e+6 cP

@Shear Rate 0.100 1/s,
Temperature 464 °F
Viscosity Test 246 cm³/g
246 cm³/g
Viscosity Number; ISO 307, 1157, 1628
Thermal Properties Metric English Comments
Melting Point 215 °C
419 °F
10°C/min; ISO 11357-1/-3
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
dry; IEC 60695-11-10
HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
dry; IEC 60695-11-10