| Category | Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive |
| Manufacturer | Devcon |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Devcon Wear Guard (High Temp) Epoxy.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.83 g/cc | 0.0662 lb/in³ |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 87 | 87 | ASTM D2240 |
| Tensile Strength, Ultimate | 31.7 MPa | 4600 psi | ASTM D638 |
| Modulus of Elasticity | 5.86 GPa | 850 ksi | In Tension; ASTM D638 |
| Flexural Yield Strength | 56.7 MPa | 8220 psi | ASTM D790 |
| Compressive Yield Strength | 91.0 MPa | 13200 psi | ASTM D695 |
| Adhesive Bond Strength | 15.9 MPa | 2300 psi | Adhesive tensile shear strength; ASTM D1002 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 49.0 µm/m-°C @Temperature 20.0 °C |
27.2 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
| Thermal Conductivity | 0.895 W/m-K | 6.20 BTU-in/hr-ft²-°F | ASTM C177 |
| Maximum Service Temperature, Air | 232 °C | 450 °F | Operating Temperature |
| Shrinkage | 0.10 % | 0.10 % | During Cure; ASTM D2566 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Constant | 38 | 38 | ASTM D150 |
| Dielectric Strength | 12.2 kV/mm | 310 kV/in | ASTM D149 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 21.1 °C | 70.0 °F | |
| Pot Life | 120 min @Temperature 23.9 °C |
120 min @Temperature 75.0 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Coverage per lb. | 60 in² | at 1/4 inch thick |
| Mix Ratio by Volume | 6 to 1 | resin:hardener |
| Mix Ratio By Weight | 13.7 to 1 | resin:hardener |