Diamond Polymers Centrex® 485 Sheet Extrusion Grade

Category Polymer , Thermoplastic , ASA Polymer
Manufacturer Diamond and Network Polymers
Trade Name Centrex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers Centrex® 485 Sheet Extrusion Grade.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Centrex 485 resin is a low-gloss, medium-impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, and it can be easily coextruded. The recommended substrate is ABS (acrylonitrile-butadiene-styrene) resin.Applications: Typical applications include those requiring weatherability and low gloss such as automotive and truck interiors, exterior siding and trim profiles. As with any product, use of Centrex 485 resin in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D792
Melt Flow 7.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
7.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 79
79
ASTM D785
Tensile Strength, Yield 20.7 MPa
3000 psi
chs 2.0 in/min; ASTM D638
Tensile Modulus 1.447 GPa
209.9 ksi
chs 2.0 in/min; ASTM D638
Flexural Strength 38.6 MPa
5600 psi
chs 0.05 in/min; ASTM D790
Flexural Modulus 1.378 GPa
199.9 ksi
tangent; chs 0.05 in/min; ASTM D790
Izod Impact, Notched 0.430 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
0.806 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
0.640 J/cm

@Thickness 3.17 mm,
Temperature -18.0 °C
1.20 ft-lb/in

@Thickness 0.125 in,
Temperature -0.400 °F
ASTM D256
1.07 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
2.00 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Impact Test 6.00 J

@Temperature -40.0 °C
4.43 ft-lb

@Temperature -40.0 °F
ASTM D3763
16.0 J

@Temperature -18.0 °C
11.8 ft-lb

@Temperature -0.400 °F
ASTM D3763
24.0 J

@Temperature 23.0 °C
17.7 ft-lb

@Temperature 73.4 °F
ASTM D3763
Thermal Properties Metric English Comments
CTE, linear 94.0 µm/m-°C
52.2 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C
174 °F
0.125";; ASTM D648
Optical Properties Metric English Comments
Gloss 10 %
10 %
Formed; 60°; ASTM D523
20 %
20 %
Sheet; 60°; ASTM D523