Material Notes:
General purpose O-ring and valve lubricant. Provides a noncuring moisture barrier; high dielectric strength; moisture and ozone resistance; good thermal, oxidation and chemical stability; suitable fore use with potable water under NSF 61. Heavy consistency, translucent white, grease-like silicone paste.Applications: Lubricating plug, sanitary, gate, ball, butterfly and automate valves, pump packing, rubber and plastic O-rings; sealing vacuum and pressure systems (especially equipment subjected to washing and harsh environments); damping medium for dash pots in electrical equipment.Base Oil: SiliconeListing/Specification: FDA, NSF 51, NSF 61Color(s): Translucent whiteThickener: SilicaNLGI#: 3 to 4Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.00 g/cc

@Temperature 25.0 °C
1.00 g/cc

@Temperature 77.0 °F
Mechanical Properties Metric English Comments
Penetration 217
217
Worked 100,000
Penetration P(60), 1/10 mm 205
205
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
399 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 2.17e+15 ohm-cm
2.17e+15 ohm-cm
Dielectric Constant 2.88

@Frequency 100 Hz
2.88

@Frequency 100 Hz
2.95

@Frequency 100000 Hz
2.95

@Frequency 100000 Hz
Dielectric Strength >= 17.7 kV/mm
>= 450 kV/in
Dissipation Factor 0.00010

@Frequency 100 Hz
0.00010

@Frequency 100 Hz
<= 0.00050

@Frequency 100000 Hz
<= 0.00050

@Frequency 100000 Hz
Arc Resistance 124 sec
124 sec
Processing Properties Metric English Comments
Shelf Life 60.0 Month
60.0 Month
Descriptive Properties Value Comments
Appearance translucent
Color white
NLGI Number 3
Water Resistant yes