Material Notes:
High strength lower durometer silicone mold making rubber, suited for the reproduction of robotic skins, tooling and immovable objects due to its thixotropic characteristics. HS III Base with HS Sprayable Catalyst Clear is recommended for use with polyesters and plaster or wax and can be used with polyurethane rigid.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc

@Temperature 25.0 °C
1.16 g/cc

@Temperature 77.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 10
10
Tensile Strength, Ultimate 2.62 MPa
380 psi
Elongation at Break 640 %
640 %
Tear Strength 19.3 kN/m
110 pli
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Descriptive Properties Value Comments
Working Time (min) 60