| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.16 g/cc | 1.16 g/cc | 23/23°C; ASTM D792 |
|
RheTech Products FRP300-01 20% Talc Reinforced Polypropylene Copolymer, Flame Retardant, Black
Applications: Electrical component housingsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Specific Gravity | 1.16 g/cc | 1.16 g/cc | ASTM D792 |
|
Polymax® Maxelast® F02-140A TPE, Halogen Free Extrusion Grade
Characteristics: Good melt strengthSoft touchSmooth surface with dry feelGood weather and heat resistanceWide range of hardnessEasy processing Halogen FreeLow smoke emissionRoHs compliantDesigned to..
|
|||
| Specific Gravity | 1.16 g/cc | 1.16 g/cc | ASTM D792 |
|
Quadrant EPP Nylatron® GSM Nylon, Cast MoS2 Filled Type 6 (ASTM Product Data Sheet) |
|||
| Specific Gravity | 1.16 g/cc | 1.16 g/cc | ISO 1183 |
|
Lehmann & Voss LUVOCOM® 1700-1401 PPO, with carbon fiber and glass fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for..
|
|||
| Specific Gravity | 1.16 g/cc | 1.16 g/cc | |
|
Momentive Performance Materials TSE 221-5U Heat Cured Rubber
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
|
|||
| Specific Gravity | 1.16 g/cc | 1.16 g/cc | ASTM D792 |
|
SABIC Innovative Plastics NORYL SE1GFN1 PPE+HIPS (Europe-Africa-Middle East)
Noryl* SE1GFN1 is a 10% glass reinforced, injection moldable modified polyphenylene ether resin. Designed for improved dimensional stability and good flow , this resin also uses non-chlorinated, non..
|
|||
| Specific Gravity | 1.16 g/cc | 1.16 g/cc | ASTM D792 |
|
SABIC Innovative Plastics NORYL SE1GFN1 PPE+PS
PPE+PS blend. 10% Glass reinforced. Non-brominated, non-chlorinated FR system. UL94 V1 listing. RTI 110/105/110. Dielectric strength. Dimensional stability. Suitable for E/E applications.
|
|||
| Specific Gravity | 1.16 g/cc | 1.16 g/cc | ASTM D792 |
|
Samsung Cheil Industries Starex® NT-7310 ABS, Unreinforced FR
Flame-retardant ABS that can be used in printer frames etc.Information provided by Samsung Cheil Industries.
|
|||
| Specific Gravity | 1.16 g/cc | 1.16 g/cc | ASTM D792 |
|
Samsung Cheil Industries Starex® TF-0956 HI-PMMA
Information provided by Samsung Cheil Industries.
|
|||
| Specific Gravity | 1.16 g/cc | 1.16 g/cc | ASTM D792 |
|
SK Chemicals SKYPEL P147D Productivity Grade
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti..
|
|||
| Specific Gravity | 1.16 g/cc | 1.16 g/cc | ASTM D792 |
|
Samsung Cheil Industries Starex® SF-0941 MABS, Unreinforced Scratch Resistant
Information provided by Samsung Cheil Industries.
|
|||
| Specific Gravity | 1.16 g/cc | 1.16 g/cc | ASTM D792 |
|
Teknor Apex Sinvicomp SHE 8500 Polyvinyl Chloride, Flexible
Availability: Asia Pacific Features: Ethylene Oxide Sterilizable Forms: Granules Processing Method: ExtrusionInformation Provided by Teknor Apex
|
|||
| Specific Gravity | 1.16 g/cc | 1.16 g/cc | ASTM D792 |
|
Lubrizol STAT-RITE® S-1100 Static Dissipative TPU
Description: Stat-Rite® S1100 is a static dissipative TPU alloy. Stat-Rite S-1100 utilizes the patented Stat-Rite inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD p..
|
|||
| Specific Gravity | 1.16 g/cc | 1.16 g/cc | ASTM D792 |
|
Chase Plastics CP Pryme® NN100MD2 (DAM) Nylon 66 with 2% MoS2 Lubricated
Information provided by Chase Plastics.
|
|||
| Specific Gravity | 1.16 g/cc | 1.16 g/cc | Mixed Adhesive |
|
Hexcel® Redux® 870 A/B Two Component Shimming and Potting Epoxy Paste Adhesive
Redux 870 A/B is a two component high performance epoxy paste adhesive, ideal for use as a Liquid Shim or for potting applications. This high temperature performing thixotropic adhesive has been spe..
|
|||
| Specific Gravity | 1.16 g/cc | 1.16 g/cc | ASTM D792 |
|
A. Schulman POLYBLAK™ 2076 Superior Black Color Concentrate, 40% Carbon Black Based In EVA
DescriptionPOLYBLAK® Black 2076 is a superior black color concentrate containing 40% carbon black in EVA. This masterbatch is designed to provide good opacity and a regular blue undertone with pig..
|
|||
| Specific Gravity |
1.16
g/cc @Temperature 25.0 °C |
1.16
g/cc @Temperature 77.0 °F |
|
|
Dow Corning HS III BASE & 10:1 COLORED CATALYST
High strength lower durometer silicone mold making rubber, suited for the detailed reproduction of fiines, art objects and similar items. HS III Base with HS III 10:1 Colored Catalyst is recommended..
|
|||
| Specific Gravity | 1.16 g/cc | 1.16 g/cc | ASTM D792 |
|
ELASTO UK Dryflex® 602700S SEBS Based Material, Filled Qualities, 70A Hardness, Black
The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material ..
|
|||
| Specific Gravity | 1.16 g/cc | 1.16 g/cc | ASTM D792 |
|
Diamond Polymers ASA TWP 155
Description: Transparent Weatherable PolymerInformation provided by Diamond Polymers, Inc.
|
|||
| Specific Gravity | 1.16 g/cc | 1.16 g/cc | Part A |
|
Epoxy Technology EPO-TEK® OM125 Optical Epoxy
Product Description: EPO-TEK® OM125 is two component, high Tg, optical epoxy designed for bonding multi-mode fiber optic connectors. Advantages & Application Notes: Color coded blue for easy operat..
|
|||
| Specific Gravity | 1.16 g/cc | 1.16 g/cc | ASTM D792 |
|
Colorite Polymers Elastichem 5011TX-02 Vinyl Compound
Description: All components in Elastichem are sanctioned by the U.S. Food & Drug Administration for food packaging applications under Title 21 of the Code of Federal Regulations. For medical use, co..
|
|||
| Specific Gravity | 1.16 g/cc | 1.16 g/cc | ASTM D792 |
|
C.O.I.M. LARIPUR® LPR2102-85AE Polycaprolactone Ester Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..
|
|||
| Specific Gravity | 1.16 g/cc | 1.16 g/cc | ASTM D792 |
|
A. Schulman POLYBATCH™ Red 5330 Concentrate Based In Polyethylene
DescriptionPOLYBATCH® 5330 is a red color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 5330 is heavy ..
|
|||
| Specific Gravity | 1.16 g/cc | 1.16 g/cc | ISO 1183 |
|
Ascend Performance Materials Vydyne® ECO-315 Nylon 66/6, non-halogenated, ignition resistant, Conditioned
Vydyne® ECO315 is non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and has an Underwriters Laboratories UL 94 fla..
|
|||
| Specific Gravity | 1.16 g/cc | 1.16 g/cc | Mixed |
|
Resinlab® UR1049 MDI Based Rigid Polyurethane Foam System
Resinlab™ UR 1049 is a, two component, water blown, 4 lb per cubic foot, MDI based rigid polyurethane foam system. It is designed to cure completely at room temperature. Being of a closed cell stru..
|
|||
| Specific Gravity | 1.16 g/cc | 1.16 g/cc | ASTM D792 |
|
PolyOne Synprene® RT-4070 Thermoplastic Elastomer - SBC, Mineral Filled
(discontinued **)
Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledApplications:Multi-PurposeMarket:AutomotiveBuilding and ConstructionIndustrialConsumer GoodsProcessing Method:ExtrusionInforma..
|
|||