Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow Corning SILASTIC® 25160 SILICONE RUBBER

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Dow Corning
Trade Name SILASTIC®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SILASTIC® 25160 SILICONE RUBBER.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
60 durometer, peroxide cured, general purpose silicone rubber compoundInformation provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc

@Temperature 25.0 °C
1.15 g/cc

@Temperature 77.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 59
59
Tensile Strength, Ultimate 9.336 MPa
1354 psi
Tensile Strength, Yield 1.62 MPa
235 psi
at 100% elongation, maximum
Elongation at Break 453 %
453 %
Tear Strength 18.2 kN/m
104 pli
Processing Properties Metric English Comments
Shelf Life 6.00 Month
6.00 Month