Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Shelf Life = 6.00 Month Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Shelf Life 6.00 Month

@Temperature -17.8 °C
6.00 Month

@Temperature 0.000 °F
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, 120 E-Glass Reinforced
Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request...
Shelf Life 6.00 Month

@Temperature 4.44 °C
6.00 Month

@Temperature 40.0 °F
Park Electrochemical Nelcote® F-555 Phenolic Prepreg, Glass Reinforced
Nelcote® F-555 is a carbon-filled MIL-R-9299 phenolic resin optimized for coating Carbonized Rayon cloth. F-555 is used extensively in the manufacture of high temperature rocket nozzles, heat shiel..
Shelf Life 6.00 Month
6.00 Month
Cartridge
Parker Chomerics Tecknit Teckfip™ FIP-C (SP) Formed in Place Conductive Elastomer
Description: This is the small particle version of the FIP-C compound. It was specifically designed for mobile cell phone applications, which require a high degree of EMI shielding. While the compou..
Shelf Life 6.00 Month

@Temperature 15.0 - 25.0 °C
6.00 Month

@Temperature 59.0 - 77.0 °F
Raschig Group MELOPLAS® 150 MF
Wood flour-reinforced MF molding compound in dark colors. High surface hardness, high mechanical strength, good electrical properties. Self-extinguishing (V-O/1,6 according to UL 94), UL-listed. Fr..
Shelf Life 6.00 Month

@Temperature 21.1 °C
6.00 Month

@Temperature 70.0 °F
From date of manufacture
Arlon 31580R020 0.020" (0.508 mm) Uncured Silicone Rubber on HDPE Carrier  (discontinued **)
Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: High Density PolyethyleneAppearance: Red silicone gum on polymer linerThis data represents typical values for the..
Shelf Life 6.00 Month

@Temperature 25.0 °C
6.00 Month

@Temperature 77.0 °F
Lord Adhesives Thermosetâ„¢ UR-329 Two Component Urethane Potting Compound
Lord UR-329 is a flexible, two-component, room temperature curing, urethane, encapsulating compound. UR-329 maintains low hardness and modulus over a wide temperature range, which imparts minimal st..
Shelf Life 6.00 Month
6.00 Month
Gwent Electronic Materials D2071120D1 Polymer Dielectric
Blue colored screen printable polymer dielectric, suitable for defining electrode areas and forms a protective layer over the electrode tracking during immersion of the electrode. The formulation i..
Shelf Life >= 6.00 Month
>= 6.00 Month
in original sealed containers at temperatures less than 40°C
Struktol VP 3735 Flame retarded epoxy resin
Applications: STRUKTOL VP 3735 is a multifunctional epoxy resin, which contains a chemically bound organophosphorous substance. Thus the mechanical properties like tenacity and modulus are not influ..
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
in original unopened containers
Master Bond MasterSil 156 Two Part, Low Viscosity Silicone
Description: Master Bond MasterSil 156 is a two component, lower viscosity silicone system for high performance potting, encapsulation and sealing. MasterSil 156 combines high temperature resistance..
Shelf Life 6.00 Month
6.00 Month
From date of manufacture
Loctite® 3607 Pin Transfer
Surface Mount AdhesivesLoctite® Chipbonder® Surface Mount Adhesives (SMAs) maintain component positioning during wave solder and solder reflow processes. Loctite offers a variety of application te..
Shelf Life 6.00 Month
6.00 Month
Dow Corning SILASTIC® LC-70-2004 PART A&B KIT
70 Durometer, 2 parts, 1 to 1 mix, translucent, FDA 21 CFR 177.2600 and BfR, XV, molding and injection molding grade Liquid Silicone Rubber. Fast curing speed, long pot life (72 hours), high transpa..
Shelf Life 6.00 Month
6.00 Month
Dow Corning 3-6006 SILICONE ADHESIVE/SEALANT
One-part, fast cure silicone adhesive.Information provided by Dow Corning
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
From date of manufacture
Arlon 28561R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 1528 FiberglassSide 2: Uncured Silicone RubberInterleave 2: PolyethyleneAppearance: Red silicone gum o..
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
From date of manufacture
Arlon 51589R015 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place of,..
Shelf Life 6.00 Month

@Temperature 21.1 °C
6.00 Month

@Temperature 70.0 °F
From date of manufacture
Arlon 55148R036 0.036" (0.914 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 2, Layer 2: Uncured Silicone Rubber Side 2, Layer 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber This data r..
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
From date of manufacture
Arlon 55609R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone Rubber LayerSide 2: Uncured Silicone RubberProduct Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass with polymer release linersThi..
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
From date of manufacture
Arlon 55900R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: 162 Style Fiberglass Appearance: Red silicone gum on glass fabricThis data represents typical values for the p..
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
From date of manufacture
Arlon CP-390C Bulk Compound
This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Di..
Shelf Life 6.00 Month

@Temperature 4.00 - 10.0 °C
6.00 Month

@Temperature 39.2 - 50.0 °F
From date of manufacture
Arlon R37230R006 0.006" (0.152 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Substrate
Design/Construction: Liner: FEP Add-on: Uncured Silicone Rubber Substrate: PTFE Coated Fiberglass This data represents typical values for the production material. The data should not be used to wri..
Shelf Life 6.00 Month
6.00 Month
Aremco Corr-Paint™ CP4010-S1 High Temperature Protective Coating, Silicone
Shelf Life 6.00 Month
6.00 Month
Aremco Corr-Paint™ CP4090 High Temperature Protective Coating Silicone, Aluminum Filled
This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a..
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
From date of manufacture
Arlon 30580R020 0.020" (0.508 mm) Uncured Unsupported Silicone Rubber on Kodacel Carrier
Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on Kodacel CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The da..
Shelf Life 6.00 Month

@Temperature 21.1 °C
6.00 Month

@Temperature 70.0 °F
From date of manufacture
Arlon 44576R009A 0.0058" (0.216 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 1165 Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene This data represents typical values for the production ma..
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
Arlon 51228R020 Silicone Rubber/Fiberglass Laminate
Interleave: 1.5 mil PE; Side 1, layer 2: uncured silicone rubber; Side 1, layer 1: Cured silicone rubber; Substrate: 7628 fiberglass; Side 2: cured silicone rubber
Shelf Life 6.00 Month

@Temperature <=23.9 °C
6.00 Month

@Temperature <=75.0 °F
From date of manufacture
Arlon R32861R006 0.0055" (0.140 mm) Uncured Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Rubber Side 2: Uncured Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, material spec..
Shelf Life 6.00 Month
6.00 Month
From date of manufacture
Arlon R33468A030 0.0305" (0.775 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured/Uncured LayersAppearance: Semi-cured blue silicone gum on glass fabricThis data Represents typical values for the production material. ..
Shelf Life 6.00 Month

@Temperature 4.44 °C
6.00 Month

@Temperature 40.0 °F
From date of manufacture
Arlon R34880T020 0.020" (0.508 mm) Uncatalyzed, Unsupported rubber on a Mylar Carrier
Design/Construction:Side 1: Uncatalyzed, Unsupported rubber on a Mylar Carrier This data Represents typical values for the production material. The data should not be used to write, or in place of, ..
Shelf Life 6.00 Month
6.00 Month
BCC Products BC 9020 Silicone RTV Rubber
BC 9020 is a violet colored, two-component, flowable compound that regardless of thickness or confinement, cures at room temperature. The cured rubber is high strength and high tear with good elonga..
Shelf Life 6.00 Month
6.00 Month
40 -90 °F
Aremco Glass-Coat™ SGC4000 High Temperature Specialty Coatings Silicone-Glass
Silicone-glass-ceramic, gray, low viscosity, scratch resistant coating for stainless steel to 900°F (482°C)
Shelf Life 6.00 Month
6.00 Month
Gwent Electronic Materials D2090124D2 Green Solder mask Dielectric
This product has been designed as a solder mask dielectric for use at high temperatures. It has been tested at 250°C and was proved to be stable for 12 weeks. Screen Printing Equipment: semi-automa..
Copyright © lookpolymers.com All Rights Reserved