Dow Corning SYL-OFF® SL 700 COATING

Category Polymer , Thermoset , Silicone
Manufacturer Dow Corning
Trade Name SYL-OFF®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SYL-OFF® SL 700 COATING.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Solvent-free, fast curing, provides extremely stable release, excellent bath stability, premium release at low peel speeds, requires catalyst additionInformation provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.970 g/cc
0.970 g/cc
Viscosity 250 cP
250 cP
dynamic
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Active Content (%) 100
Appearance clear liquid
Solvent solventless