Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow Saran® 18L-WP White Plastic Barrier Film

Category Polymer , Film , Thermoplastic , PVDC
Manufacturer Dow Chemical
Trade Name Saran®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Saran® 18L-WP White Plastic Barrier Film.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Saran™ 18L-WP is a white biaxially oriented monolayer barrier film, preshrunk for lamination applications. It is available in 75 gauge, as single or double wound rolls.Information provided by Dow
Physical Properties Metric English Comments
Water Vapor Transmission 7.20 g/m²/day
0.464 g/100 in²/day
at 100°F, 90% RH; ASTM F1249-90
Oxygen Transmission 0.512 cc-mm/m²-24hr-atm
1.30 cc-mil/100 in²-24hr-atm
10% RH; ASTM D3985
Thickness 19.0 microns
0.750 mil
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 80 %
80 %
ASTM D882
Film Elongation at Break, TD 75 %
75 %
ASTM D882
Secant Modulus, MD 0.5171 GPa
75.00 ksi
2% Secant; ASTM D882
Secant Modulus, TD 0.4826 GPa
70.00 ksi
2% Secant; ASTM D882
Coefficient of Friction, Dynamic 0.15
0.15
Film to Metal; ASTM D1894
Film Tensile Strength at Break, MD 82.7 MPa
12000 psi
ASTM D882
Film Tensile Strength at Break, TD 110 MPa
16000 psi
ASTM D882
Thermal Properties Metric English Comments
Shrinkage, MD 11 %
11 %
Unrestrained, 100°C Air; ASTM D1204
Shrinkage, TD 4.0 %
4.0 %
Unrestrained, 100°C Air; ASTM D1204
Optical Properties Metric English Comments
Gloss 40 %
40 %
45°; ASTM D2457
Transmission, Visible 0.20 %
0.20 %
Clarity; ASTM D1746
Descriptive Properties Value Comments
Yield in2/lb 21600
Calculated
Users viewing this material also viewed the following: