Material Notes:
Saran™ 506 Polymer is designed as an ignition resistant adhesive bonding agent. Saran™ 506 is a vinylidene chloride copolymer supplied as a white, micronized powder. It is unaffected by humidity, and has outstanding adhesion to fibrous substrates. No expressed data on flammability are to be considered indications of behavior of this material in actual fire situations; virtually all organic materials burn when sufficient heat and oxygen are supplied.Information provided by Dow
Physical Properties Metric English Comments
Bulk Density 0.400 - 0.561 g/cc
0.0145 - 0.0203 lb/in³
Dow Method
Particle Size 15 - 25 µm
15 - 25 µm
Dow Method
Thermal Properties Metric English Comments
Melting Point 114 - 172 °C
237 - 342 °F
Dow Method (DSC)
Oxygen Index 63 - 77 %
63 - 77 %
ASTM D2863
Optical Properties Metric English Comments
Optical Density 0.26 - 2.6
0.26 - 2.6
[D<sub>m</sub>]; Flaming Mode; NBS Chamber
0.33 - 2.93
0.33 - 2.93
[D<sub>m</sub>]; Smoldering Mode; NBS Chamber