Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Kalrez® 1045 Fluoroelastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer DuPont Performance Polymers (Former DuPont Elastomers)
Trade Name Kalrez®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Kalrez® 1045 Fluoroelastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
DuPont™ Kalrez® 1045 perfluoroelastomer parts are a specialty white product that is reinforced with a mineral filler that is highly resistant to oxidizing environments (carbon black-filled products may be affected by black degradation in oxidizing media). Typical applications include sealing rocket propellants, hot oxidizing acids, wet halogens and halogenated gases. A maximum continuous service temperature of 260 C (500 F) is suggested. Performance Features/Benefits: Excellent resistance to highly oxidizing media, i.e., nitrogen tetroxide (N2O4), etc. Excellent resistance to hot oxidizing acids, i.e., red fuming nitric, etc., wet halogens and halogenated gases Good mechanical strength properties Good thermal stability Good compression set resistance
Mechanical Properties Metric English Comments
Hardness, Shore A 77
77
ASTM D2240
Tensile Strength at Break 15.16 MPa
2199 psi
ASTM D412
Elongation at Break 150 %
150 %
ASTM D412
100% Modulus 0.00827 GPa
1.20 ksi
ASTM D412
Compression Set 30 %

@Temperature 204 °C,
Time 252000 sec
30 %

@Temperature 399 °F,
Time 70.0 hour
ASTM D395B
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
DuPont Test Method
Descriptive Properties Value Comments
Color White